Eyelets and Rivets for Panel and Board Fixing
Product Specifications
Product Overview
An eyelet is a brass tube with a flange at one end. It goes through a hole in a board or a panel, and a staking tool rolls the plain end over so the flange and the roll trap the material between them. What the eyelet does is line the hole: a screw, a pin or a wire can then pass through without cutting into the board, and the load is spread over the flange instead of sitting on a bare drilled edge. On a single sided board the eyelet also gives a solderable pad a mechanical anchor, which is why it turns up on terminal footprints and on connectors that take a side load.
The length is the figure that gets chosen wrong. The rule on the maker data is to add 0.040 in (1.00 mm) to the total assembly thickness and then take the next length that is available. The worked example from the catalogue is short: for a 1/16 in board with a 0.020 in terminal, 0.020 + 0.062 + 0.040 comes to 0.122 in, so the 0.125 in eyelet is the one that fits. A part chosen by eye at the same hole size is usually one step short, and a short eyelet either will not roll or rolls onto the flange and splits.
The bore and the flange follow the job rather than the hole. The small group has a 0.059 in barrel outside diameter with a 0.045 in bore and a 0.125 in flange, which is the size for a 0.105 in hole, drilled with a #51. The middle group runs a 0.089 in barrel, a 0.070 in bore and a 0.150 in flange for a 0.093 in hole, which is a #42 drill. The heavy group has a 0.121 in barrel, a 0.102 in bore and a 0.200 in flange for a 0.125 in hole, which is a #30 drill, and the largest group has a 0.156 in barrel with a 0.132 in bore and a 0.245 in flange for a 5/32 in hole.
Material is brass with a bright electro tin plate to MIL-T-10727, which is the finish that keeps a brass eyelet solderable and keeps the surface from tarnishing in a box that sits on a shelf for a year. The staking tools are matched to the group and are sold as a top and bottom pair in tool steel: 3075 for the 0.059 in barrel, 3076 for the 0.089 in barrel, 3077 for the 0.121 in barrel and 3079 for the 0.156 in barrel. Using the wrong pair is the second most common way an eyelet fails, because a tool for a larger bore rolls the flange before the tube has come through the panel.
Rivets are the other half of the page, and nylon snap rivets are the easiest version to specify because they need no tooling at all. The part is pressed into the hole and the split shank opens behind the panel. The 3440 covers a panel stack from 0.051 to 0.079 in with a 0.130 in length and a 0.085 in hole, and the range runs up to the 3450 at 0.295 to 0.335 in of panel with a 0.390 in length. They are Nylon 6/6 rated UL 94V-2, black, and they work from -20 to 60 C. Because they press in from one side and can be levered out again, they suit a cover, a light bracket or a fan guard, and they are not the part for a joint that carries load or sees heat.
The practice points are short. Deburr the hole before staking, because a burr under the flange holds the eyelet off the surface and the roll then sits proud. Support the back of a thin panel when a rivet goes in, or the panel dishes and the head stands off. And keep the staking tool set to the group, not to the job, because a tool that is adjusted deeper to suit one panel will split the next part on the same bench.
Key Specifications
| Parameter | Value | Applies to |
|---|---|---|
| Eyelet material | Brass, bright electro tin to MIL-T-10727 | All brass eyelets |
| Barrel outside diameter | 0.059, 0.089, 0.121, 0.156 in | By group |
| Barrel bore | 0.045, 0.070, 0.102, 0.132 in | By group |
| Flange diameter | 0.125, 0.150, 0.200, 0.245 in | By group |
| Length under flange | 0.062 to 0.250 in | By part |
| Mounting hole | 0.105 in (#51), 0.093 in (#42), 0.125 in (#30), 5/32 in | By group |
| Length selection rule | Add 0.040 in to the assembly thickness, take the next length | All eyelets |
| Staking tools | 3075, 3076, 3077, 3079, top and bottom pair | By group |
| Tool material | Tool steel, polished | All staking tools |
| Snap rivet material | Nylon 6/6, UL 94V-2, black | 3440 to 3450 |
| Snap rivet panel stack | 0.051 to 0.335 in | By part |
| Snap rivet length | 0.130 to 0.390 in | By part |
| Snap rivet mounting hole | 0.085, 0.144, 0.163 in | By group |
| Snap rivet temperature | -20 to 60 C | 3440 to 3450 |
| Snap rivet installation | Press in from one side, no tooling, removable | 3440 to 3450 |
Included Models and Order Codes
The rows below are the eyelets we quote most often. Length under the flange, flange diameter and mounting hole are given per part, because the stack and the hole are what decide the fit, and a dash means the maker does not publish that figure.
| Part Number | Barrel OD | Bore | Length Under Flange | Flange | Mounting Hole | Staking Tool |
|---|---|---|---|---|---|---|
| 22 | 0.059 in | 0.045 in | 0.062 in | 0.125 in | 0.105 in, drill #51 | 3075 |
| 24 | 0.059 in | 0.045 in | 0.125 in | 0.125 in | 0.105 in, drill #51 | 3075 |
| 26 | 0.059 in | 0.045 in | 0.187 in | 0.125 in | 0.105 in, drill #51 | 3075 |
| 33 | 0.089 in | 0.070 in | 0.093 in | 0.150 in | 0.093 in, drill #42 | 3076 |
| 34 | 0.089 in | 0.070 in | 0.125 in | 0.150 in | 0.093 in, drill #42 | 3076 |
| 35 | 0.089 in | 0.070 in | 0.156 in | 0.150 in | 0.093 in, drill #42 | 3076 |
| 36 | 0.089 in | 0.070 in | 0.187 in | 0.150 in | 0.093 in, drill #42 | 3076 |
| 44 | 0.121 in | 0.102 in | 0.125 in | 0.200 in | 0.125 in, drill #30 | 3077 |
| 46 | 0.121 in | 0.102 in | 0.187 in | 0.200 in | 0.125 in, drill #30 | 3077 |
| 48 | 0.121 in | 0.102 in | 0.250 in | 0.200 in | 0.125 in, drill #30 | 3077 |
| 15 | 0.156 in | 0.132 in | 0.156 in | 0.245 in | 5/32 in | 3079 |
Nylon Snap Rivets for Cover and Bracket Joints
Snap rivets press in from one side and can be levered out again, so they suit a cover or a guard that may come off. Panel stack, length and hole size are given per part because those three figures decide whether the rivet grips or rattles.
| Part Number | Panel Stack | Rivet Length | Rivet Diameter | Head Diameter | Mounting Hole |
|---|---|---|---|---|---|
| 3440 | 0.051 to 0.079 in | 0.130 in | 0.076 in | 0.165 in | 0.083 to 0.087 in |
| 3441 | 0.083 to 0.110 in | 0.160 in | 0.076 in | 0.165 in | 0.083 to 0.087 in |
| 3444 | 0.146 to 0.181 in | 0.240 in | 0.138 in | 0.252 in | 0.142 to 0.146 in |
| 3445 | 0.177 to 0.217 in | 0.280 in | 0.138 in | 0.252 in | 0.142 to 0.146 in |
| 3447 | 0.177 to 0.217 in | 0.280 in | 0.158 in | 0.315 in | 0.161 to 0.165 in |
| 3449 | 0.256 to 0.295 in | 0.350 in | 0.158 in | 0.315 in | 0.161 to 0.165 in |
| 3450 | 0.295 to 0.335 in | 0.390 in | 0.158 in | 0.315 in | 0.161 to 0.165 in |
Key Features
Length rule stated with an example – Adding 0.040 in to the assembly thickness and taking the next length is worked through on a 1/16 in board, so the part is chosen from the stack rather than from the hole.
Four barrel groups – 0.059, 0.089, 0.121 and 0.156 in barrels cover a 0.105 in hole up to a 5/32 in hole, with the flange and the drill size listed for each.
Staking tool per group – 3075, 3076, 3077 and 3079 are matched to the barrel size and sold as a top and bottom pair, which is how a roll gets formed without splitting the flange.
Solderable tin finish – Brass with a bright electro tin plate to MIL-T-10727 keeps the eyelet solderable and stops the surface tarnishing in storage.
Rivets with no tooling – Nylon snap rivets press in from one side and come out again, so a cover or a fan guard is fitted on the line without a press.
Hole sizes given as drill numbers – #51, #42, #30 and 5/32 in are listed with the imperial figure, because a drill chart and a drawing rarely use the same units.
Applications
These parts are used where a hole has to be lined, a thin panel has to take a screw, or two light panels have to be held together without a thread.
Terminal and connector footprints – A 0.089 in brass eyelet in a 0.093 in hole gives a connector tab a metal seat and a solderable pad that will not lift under a side load.
Front panel labels and plates – A 0.125 in eyelet under a 0.200 in flange holds a small plate against a 1.6 mm panel without crushing the print around the hole.
Covers, guards and fan grilles – A 3445 snap rivet holds a 4 mm cover stack and comes out again with a lever, which is what a serviceable cover needs.
An eyelet or a rivet is picked against the hole in the panel, so the drill size is checked against the SUPERB PCB mounting drawing before the first part is staked. On the SUPERB PCBA route a brass eyelet is staked into a terminal footprint after the board is assembled, and the tool is set so the flange sits flat without crushing the pad ring.
Sourcing and Cross-Reference
An eyelet is bought by hole and by stack. The barrel size follows the hole, but the length follows the total thickness of everything that goes through it, and that is the number a drawing often leaves out. When an eyelet is replaced on a board that is already qualified, the mounting hole and the length under the flange are the two figures to check first, because a 0.187 in part in a 0.125 in stack will not roll and a 0.093 in part in a 0.125 in stack will split.
The second point is the tool. Staking tools are matched to the barrel group and are not adjustable for depth on the fly, so a bench that runs two eyelet sizes needs two tool sets. A tool that is set deeper to suit a thick panel will roll the flange of the next part on the same bench, and that failure looks like a bad eyelet rather than a bad setup.
The third point is the choice between an eyelet and a rivet. An eyelet lines a hole for something else to pass through, and it holds a light plate. A rivet joins two panels and carries load. On a cover that has to come off, a nylon snap rivet is the right part; on a bracket that has to stay put, a staked brass eyelet with a screw through it is the one that survives vibration. We quote the eyelets, the rivets and the staking tools as one set, because they are ordered together and fitted by the same operator.
SUPERB Assembly stakes one eyelet into a scrap panel at the start of a run and pulls it against the flange, because a staking tool set a quarter turn too deep splits the roll and the eyelet looks seated until the screw is tightened.
Q: Can you supply brass eyelets for a 1.6 mm board with a 0.093 in hole, and confirm the length under the flange and the staking tool number?
A: Send the panel thickness, the hole size and the screw or pin that goes through the eyelet. The SUPERB Tech desk quotes the eyelet with its length under the flange, because the rule on this page is to add 0.040 in to the assembly thickness and take the next longer part, and a part chosen by eye is usually one size short.
Why Buy Eyelets and Rivets Through SUPERB
- Stack checked before length: The eyelet is quoted against the total thickness, which is where a 0.125 in part gets ordered for a 0.187 in stack.
- Hole and drill size stated: Each group carries its mounting hole and drill number, so the panel is drilled to the part rather than the part being forced into the hole.
- Tool quoted with the part: The staking tool is quoted with the eyelet, because a box of correct parts and the wrong tool set is a run of split flanges.
- Brass with a solderable finish: The tin plated brass parts take solder and hold up in storage, which matters on a board that is built in batches.
- Rivets on the same page: The snap rivets cover the joints that have to come apart, so a cover and a bracket are not forced onto the same fastener.
Related Product Families
This page is part of the component range we supply for industrial, telecom, medical and defence builds. Continue with: Standoffs Spacers and Mounting Hardware for Board Stacks, Threaded Inserts and Standoff Nuts for Plastic Enclosures, Nylon Grommets and Hole Plugs for Panel Openings, Turret Terminals and Solder Lugs for Panel Wiring, EMI Shielding Cans and Contact Gaskets for RF Boards, How to Verify a Drop in Replacement.