Solder is a material decision before it is a process decision. The alloy sets the melting point and the joint strength, the flux class sets what has to be cleaned and what the inspection sheet has to record, and the form sets which machine or which hand applies it. Get the alloy wrong and the joint fails a thermal cycle; get the flux class wrong and the board fails a cleanliness test after it has passed every electrical check.
The two alloys on this page are the two that most assemblies use. SAC305 is Sn96.5 Ag3.0 Cu0.5, lead free, with a melting range of 217 to 219 C, a density of 7.37 grams per cubic centimetre and a hardness of 14.1 HV on the Kester data sheet. Sn63Pb37 is the eutectic tin lead alloy at 183 C, which is 35 degrees lower and therefore kinder to a hand iron, a heat sensitive part and a rework bench. A lead free build uses SAC305; a legacy build that is exempt, or a repair of an existing leaded board, uses Sn63Pb37.
The alloy also sets the process window. On a wave or selective machine, SAC305 wants a pot temperature of 255 to 265 C for wave soldering and 280 to 320 C for selective soldering, and the data sheet notes that a nitrogen blanket below 1000 ppm oxygen reduces oxidation further. A leaded pot runs lower, which is one reason a mixed shop keeps the two baths separate rather than sharing a pot and a pump.
Flux class is written as a J STD 004 code, and the code is the whole specification. A no clean flux is ROL0 or ROL1 depending on the halide content, and it is left on the board. A water soluble flux is ORM0 or ORH1 and has to be washed, which means the assembly needs a wash line and a drying step. An RMA or an RA flux sits between the two. The solder wire on this page is offered in all four chemistries, and the part number changes with the core: the 245 core is no clean, 331 is water soluble, 285 is RMA and 44 is RA.
Wire diameter follows the joint, not the operator's preference. 0.015 in is for a fine pitch rework and a 0402 part, 0.020 in and 0.025 in for general hand soldering, 0.031 in for a through hole joint and a connector tail, and 0.050 in and 0.062 in for a ground plane, a shield can or a heavy lug where the iron needs to deliver heat quickly. The core percentage, 50, 58 or 66, is the flux by weight, and a 66 core leaves more residue for the same length of wire.
Paste is the stencil form. On the Kester EP256 no clean paste the metal content is 90 percent, the powder is Type 3 as standard, the stencil life is eight hours or more and the shelf life is six months at 0 to 10 C. The same data sheet gives a printing speed to 200 mm per second, a stencil printing downtime of up to 90 minutes with an effective first print down to 20 mil, and a classification of ROL0 or ROL1 depending on the revision. EP256 is offered in Sn63Pb37, Sn62Pb36Ag2 and Sn43Pb43Bi14.
A lead free paste for the same stencil is a different part. Kester NXG1 is a no clean ROL1 paste in SAC305 Type 3, supplied in a 500 gram jar or a 600 gram cartridge, and it is the one to specify when the board has an OSP finish and the paste has to sit on the pad through a shift. For a fine pitch part below 0.4 mm the powder moves to Type 4, which is a different part number rather than a setting on the printer.
Preforms are the third form, and they exist for a joint that neither wire nor paste can reach. A preform is a shaped piece of solder, a washer, a ring, a disc or a rectangle, placed in the joint and reflowed, with or without a flux coating. It is the standard answer to a seam that has to be filled with a controlled volume, a shield can that has to be sealed to a ground ring, or a connector body that has to be soldered to a pad without a stencil. Preforms are quoted by alloy, shape and volume, because the shape is drawn to the joint.
Storage is part of the material. Paste is held at 0 to 10 C and stabilised at room temperature before printing, wire is held in a dry store, and a spool that has been open for a season is checked for oxidation before it goes back on the line. A paste jar that was left out over a weekend prints with a different slump, and the defect it produces, a bridge on a 0.5 mm pitch part, is blamed on the stencil rather than on the jar.
Key Specifications
| Parameter | Value | Notes |
|---|---|---|
| Alloys | SAC305 and Sn63Pb37, plus Sn62Pb36Ag2 paste | Lead free and leaded |
| SAC305 composition | Sn 96.5, Ag 3.0 plus or minus 0.2, Cu 0.5 plus or minus 0.1 | Lead 0.07 percent maximum |
| Melting range | 217 to 219 C on SAC305, 183 C on Sn63Pb37 | The gap sets the process window |
| Density | 7.37 grams per cubic centimetre on SAC305 | Per the alloy data sheet |
| Wave solder pot temperature | 255 to 265 C on SAC305 | Selective 280 to 320 C |
| Wire diameters | 0.015 in to 0.062 in | Seven sizes on the page |
| Flux core | 50, 58 and 66 percent by weight | Core code changes the part number |
| Flux classes | No clean ROL0 and ROL1, water soluble ORM0, RMA and RA | Per J STD 004 |
| Paste metal content | 90 percent | Stencil printing and enclosed head |
| Paste powder | Type 3 standard, Type 4 for fine pitch | Per J STD 005 |
| Paste stencil life | 8 hours or more | Downtime to 90 minutes |
| Paste shelf life | 6 months at 0 to 10 C | Stabilise at room temperature before use |
Included Models and Order Codes
Wire part numbers are the Kester 24 series with the alloy and the flux core in the number, and the paste part numbers are quoted with their alloy and powder type. A part number that does not state the core is not a complete order.
| Part Number | Form | Alloy | Flux Class | Size | Notes |
|---|---|---|---|---|---|
| 24-6337-8807 | Wire, 1 lb spool | Sn63Pb37 | No clean, 245, 50 core | 0.020 in | General hand soldering |
| 24-6337-8809 | Wire, 1 lb spool | Sn63Pb37 | No clean, 245, 50 core | 0.025 in | Fine pitch and rework |
| 24-6337-8800 | Wire, 1 lb spool | Sn63Pb37 | No clean, 245, 50 core | 0.031 in | Through hole joints |
| 24-6337-8801 | Wire, 1 lb spool | Sn63Pb37 | No clean, 245, 58 core | 0.031 in | More flux for an oxidised pad |
| 24-6337-8802 | Wire, 1 lb spool | Sn63Pb37 | No clean, 245, 66 core | 0.031 in | Heavy residue, strong wetting |
| 24-6337-8813 | Wire, 1 lb spool | Sn63Pb37 | No clean, 245, 50 core | 0.040 in | Connector tails |
| 24-6337-8814 | Wire, 1 lb spool | Sn63Pb37 | No clean, 245, 50 core | 0.050 in | Ground plane and lugs |
| 24-6337-8817 | Wire, 1 lb spool | Sn63Pb37 | No clean, 245, 50 core | 0.062 in | Shield can and heavy lug |
| 24-6337-6401 | Wire, 1 lb spool | Sn63Pb37 | Water soluble, 331, 66 core | 0.020 in | Needs a wash line |
| 24-6337-9702 | Wire, 1 lb spool | Sn63Pb37 | RMA, 285, 66 core | 0.020 in | Repair of an existing board |
| 24-7068-7603 | Wire, 1 lb spool | SAC305 | No clean, 58 core | 0.020 in | Lead free rework |
| 24-7068-7601 | Wire, 1 lb spool | SAC305 | No clean, 58 core | 0.031 in | Lead free through hole |
| 24-7068-7606 | Wire, 1 lb spool | SAC305 | No clean, 58 core | 0.050 in | Lead free heavy joint |
| 24-7068-7607 | Wire, 1 lb spool | SAC305 | No clean, 58 core | 0.062 in | Lead free shield can |
| Kester SAC305 bar | Bar, 1 kg and 20 kg | SAC305 | For wave and selective | Bar | Pot 255 to 265 C |
| Kester EP256 | Paste, jar or cartridge | Sn63Pb37, Sn62Pb36Ag2, Sn43Pb43Bi14 | No clean ROL0, 90 percent metal | Type 3 | Stencil life 8 h |
| Kester NXG1 | Paste, 500 g jar or 600 g cartridge | SAC305 | No clean ROL1, 90 percent metal | Type 3 | Lead free, OSP compatible |
| Solder preform | Washer, ring, disc or rectangle | SAC305 or Sn63Pb37 | Bare or flux coated | Drawn to the joint | Volume set by the shape |
Key Features
Two alloys, one process sheet – SAC305 at 217 to 219 C and Sn63Pb37 at 183 C, so a lead free build and a repair are quoted from the same page.
Flux class as a part number – No clean, water soluble, RMA and RA are separated in the number, so the cleanliness requirement follows the material.
Wire diameter by joint – 0.015 in to 0.062 in, with the through hole, fine pitch and heavy lug cases listed against their size.
Core percentage stated – 50, 58 and 66 core, because the flux weight decides the residue and the wetting on an oxidised pad.
Paste with a real shelf life – 90 percent metal, Type 3 powder, eight hour stencil life and six months at 0 to 10 C on the data sheet.
Type 4 for fine pitch – A different powder for a part below 0.4 mm, quoted as its own part rather than as a printer setting.
Preforms for the joint nothing else reaches – A seam, a shield ring or a connector body soldered with a controlled volume in a shape drawn to the joint.
Applications
These materials go on hand soldering benches, stencil printers, wave and selective machines and rework stations, on boards with a HASL, ENIG or OSP finish.
Through hole and connector soldering – 0.031 in no clean wire on a connector tail, with the iron set for the alloy rather than for the part.
SMT reflow on a stencil line – Type 3 no clean paste at 90 percent metal on a 0.5 mm pitch board, with the stencil life tracked against the shift.
Rework and repair – 0.020 in wire and a small paste jar at the rework bench, with the alloy matched to the board being repaired and not to the new build.
Shield can and connector seams – A preform ring or a drawn shape that fills the seam with a fixed volume, on a joint a stencil cannot reach.
Solder is chosen by alloy, flux and form together, and the alloy has to agree with the finish on the board that the SUPERB PCB process sheet specifies. On the SUPERB PCBA line the wire and the paste are kept in separate controlled stores, because a leaded wire on a lead free build is a contamination that shows up as a failed ion chromatography test weeks later.
Sourcing and Cross-Reference
Solder is quoted by alloy, flux class and form. The alloy has to match the board finish and the process temperature, the flux class has to match the cleaning step that the assembly actually has, and the form has to match the machine. A quotation that names only the alloy is a quotation that will come back for the other two.
Where an alloy is being changed, the profile changes with it. Moving a reflow profile from Sn63Pb37 to SAC305 means a peak near 235 to 245 C and a longer soak, and a board that was profiled for the leaded paste will not wet on the same setting. We quote the paste and the profile reference together so the change is one step.
For a discontinued part or a flux that is being withdrawn, the substitute is matched on alloy, flux class and powder type. The alloy is not negotiable, the flux class can move within the same cleaning strategy, and the powder type is fixed by the finest pitch on the board. We check all three before we quote an alternative.
SUPERB Assembly records the lot number of every wire spool and every paste jar against the work order, and checks the paste against its refrigeration log before the stencil is loaded, because a jar that has been out of the fridge for a shift prints differently in the afternoon.
Q: Can you supply SAC305 no clean wire in 0.031 in and Type 3 paste in the same order, and confirm the flux class and the storage conditions for both?
A: Send the alloy, the flux class, the wire diameter or the paste powder type, the board finish and the process temperature. The SUPERB Tech desk quotes the wire, the paste or the preform with its alloy and its flux class, so the process sheet and the material agree.
Why Buy Solder Through SUPERB
- Alloy, flux and form quoted together: A part number that names only the alloy is not an order, so the three are confirmed before the quotation goes out.
- Leaded and lead free side by side: SAC305 and Sn63Pb37 wire, paste and preforms, so a repair and a new build are served from one desk.
- Flux class stated per part: No clean, water soluble, RMA and RA with the J STD 004 code, which is what the cleanliness test references.
- Storage and shelf life published: Paste at 0 to 10 C for six months and a stencil life of eight hours, so the store is planned rather than guessed.
- Small quantities for a rework bench: A single spool or one paste jar is quoted without a case quantity, which suits a service depot.
Related Product Families
This page is part of the component range we supply for industrial, telecom, medical and defence builds. Continue with: Butt Splices and Crimp Connectors for Wire Joins, Heat Shrink Tubing and Sleeves for Harness Protection, EMI Shielding Cans and Contact Gaskets for RF Boards, Test Points and Spring Contacts for Board Probing, Fuse Holders and Clips for Board Level Protection, BOM Shortage Recovery.