Contact Us

PCBA Inspection Before Shipment

PCBA Inspection Before Shipment

PCBA Inspection Before Shipment

A PCBA passes or fails on facts that are mostly invisible: a joint under a BGA, a component placed one pad over, a via that voided during reflow, a connector that will crack in the third thermal cycle at the customer site. None of these are visible at final visual inspection, and all of them are cheaper to find in our building than in yours.

This page covers the sequence we run between the last reflow and the packing bench, why the order of the stations matters, and what a batch has to show before it is released.

Why the sequence matters

The stations are not interchangeable and they are not a menu. Each one answers a question the previous one cannot:

  • SPI asks whether the paste was placed correctly, before the parts are on the board. It is the only station that can catch a stencil or printer problem while it is still cheap.
  • AOI after reflow asks whether every part is present, oriented and wetted. It cannot see under a package.
  • X-ray asks what is under the package: BGA voiding, head-in-pillow, opens hidden by the body, and the fill condition of through-hole joints.
  • ICT asks whether the assembled circuit is electrically what the netlist says, independent of how it looks.
  • FCT asks whether the board does its job with power applied and signals at the pins, which is the question the customer actually cares about.

Run them out of order and the yield data stops being diagnostic: a failure at FCT that should have been caught at ICT turns into a debugging session instead of a rework instruction.

The stations

StationWhat it catchesCoverage
Solder paste inspection (SPI)Volume, area and height deviation, bridging, insufficient paste on fine pitch100 percent of printed boards
AOI after reflowMissing, reversed, offset or tombstoned parts, insufficient or excess solder, polarity100 percent, with programmed libraries per product
X-ray inspectionBGA voiding and bridging, head-in-pillow, QFN thermal pad voids, through-hole fillFirst article plus sampling per shift, 100 percent on safety-critical builds
In-circuit test (ICT)Opens, shorts, wrong or missing values, reversed diodes, unprogrammed partsBed-of-nails at volume, flying probe for prototypes and low volume
Functional test (FCT)Behaviour with power and signals applied: rails, clocks, communication, sensor response100 percent where a fixture exists
Boundary scan / JTAGInterconnect opens on fine-pitch BGA nets that no probe can reachWhere the design provides access
Burn-in and agingEarly-life failures, thermal drift, intermittent joints that pass a cold testPer specification, typically 8 to 48 hours at elevated temperature
CleanlinessIonic residue from flux and handling, which shows up later as leakage or corrosionPer lot by ROSE extraction
Final visual and dimensionalCoating, label, connector seating, damage, warpage100 percent

Environmental and reliability testing

Functional test proves the board works today. Environmental testing asks whether it will still work after the conditions it is going to meet, and it is the part of the release that most often gets skipped because it takes time rather than because it is difficult.

  • Temperature and humidity. Soak at the upper and lower operating limits, and damp heat where condensation is a realistic field condition. The failure modes to watch are connector intermittency, coating integrity and drift in analogue references.
  • Thermal cycling. The test that finds CTE mismatch: BGA corner joints, press-fit pins, heavy copper interfaces. A board that passes one cycle and fails two hundred is a field return waiting to happen.
  • Vibration and mechanical shock. Relevant to anything that moves: vehicle, drone, machine tool, portable instrument. Fixturing matters as much as the profile, so the test report has to state the mounting as well as the g-levels.
  • Accelerated life testing. Higher stress for a shorter time, used to compare design variants or to estimate a failure distribution, not to declare a lifetime from a single sample.

These are run per the customer's specification or per the standard the product is being qualified against, and the report states the profile, the sample size and the failure criterion, because a pass without those three numbers means nothing.

First article and batch release

Two different decisions, two different records.

The first article is the full sequence on the first boards off the line: SPI, AOI, X-ray with void measurement, ICT, FCT, and a dimensional check against the drawing. It is signed before the batch continues, and any change to stencil, paste, profile, component supplier or layout restarts it.

The batch release is what travels with the shipment: the AOI and ICT pass counts against the quantity, the X-ray images for the sampled boards, the FCT results with the test limits, the burn-in record where specified, the cleanliness result, and the final visual result with inspector and date.

Packing is part of the inspection

A board that passes every station and arrives with a cracked connector is a failed shipment. Before the carton is closed we check ESD bagging, moisture barrier where required, desiccant, mechanical protection around connectors and tall parts, and the label against the packing list. Where the customer has a packaging specification, that specification is the acceptance criterion, not our default.

What to send us

For an assembly quote we need the BOM, the Gerber set, the assembly drawings and the test specification if you have one. If you do not have a test specification, we will propose one based on the board's function and tell you what each station adds to the cost, so the decision is yours rather than buried in a price.

Email pcba@superb-tech.com or WhatsApp +86 133 9608 1443 with your files.

The two gates before this one

Assembly is the last gate, not the only one. Component inspection decides whether the parts entering the line are what the label says, and PCB inspection decides whether the bare board meets IPC-6012 before any part is placed.