Contact Us

Depanelization Methods

Depanelization Methods

The panel is agreed early, when the array is drawn and the rail width is set. The way it comes apart is usually agreed at the same meeting, by habit, and then it is fixed: tooling follows the choice, and changing it later means new tooling and a new first article.

Depanelization methods differ in three things that matter to a buyer: what the edge looks like after separation, how much stress the board takes while it separates, and what the method costs once the volume is known. None of the four common methods wins on all three, which is why the choice belongs to the board and not to the shop.

Four ways a panel comes apart

V-score, tab routing, break-away tabs with perforations, and laser separation. Each is a different answer to the same question: how do two boards that were made as one become two boards without damaging either. A fifth method, sawing, still exists for straight cuts on thick material, and is rare outside that case.

V-score: straight lines and speed

A V-score cuts a groove on both faces along a straight line and leaves a web that is broken after assembly. We work to a residual of 0.25 to 0.50 mm with 0.10 mm tolerance, angles of 30, 45 or 60 degrees, up to 30 cuts per panel and a board width of 60 to 480 mm.

It is the fastest method per panel and the cheapest in tooling, and it has one hard limit: every cut is a straight line across the whole panel. A board with a curved outline, a cut-out or a connector that overhangs the score line cannot use it. The web also leaves a visible groove on both faces of the finished board, which matters on a visible edge and does not matter inside a housing.

Tab routing: any outline, one board at a time

A router follows the outline with a milling bit and leaves short tabs that hold the board until they are cut. Any shape is possible, including curves, internal cut-outs and boards that share an edge with a connector. The edge is clean and square, with no groove on either face.

The cost is time. Routing is a per-panel operation with a tool path, so it is slower than scoring and it needs clearance around the bit, which is part of why a routed panel needs a wider rail. The router also leaves dust, which matters on a board with open cavities or a sensitive finish.

Break-away tabs and hand snapping

Perforations along a tab let an operator snap the board out by hand. The tooling is nearly free, there is no machine time, and it suits small runs and prototypes where the edge does not show. What it leaves is a row of nibs on the edge and a rough break line, and the snap is uncontrolled: the same panel breaks one way for one operator and another way for the next.

Hand snapping is also the method that puts the most local stress into the board, right beside the break line. Parts placed near that line take it.

Laser separation

A laser cuts without a mechanical tool touching the board, which removes the bending stress entirely. It suits thin boards, flex and rigid-flex, fine pitch parts placed close to the outline, and any case where the edge cannot take a groove or a nib. It is the slowest method per panel and the most expensive per unit at volume, so it is chosen for the boards that need it rather than as a default.

The cut edge is different from a routed edge: there is a heat affected zone and some soot, which has to be cleaned before conformal coating or wire bonding.

What each method does to the board

MethodEdge after separationStress into the boardBest fit
V-scoreGroove on both faces, straight onlyBending along the web when the panel is brokenRectangular arrays, high volume, edge hidden
Tab routingClean and square, any shapeLow, concentrated at the tabsCurved outlines, cut-outs, connectors at the edge
Break-away tabsNibs and a rough break lineHigh and local, at the snap lineSmall runs, prototypes, edge not visible
LaserCut edge with heat affected zoneNone mechanicalThin board, flex, parts close to the outline

Thickness and warpage decide more than habit

We run 0.6 to 3.2 mm on the standard line, and the two ends behave differently. A thin board scores easily and breaks with little force, and it also flexes more during assembly, where the limit we hold is 0.75 percent warpage for SMT. A thick board needs a deeper score to break cleanly, and a heavy copper layer makes the web harder to control.

A board that is already close to the warpage limit is a poor candidate for a method that bends it. That is the point where the separation choice and the flatness requirement meet, and it is cheaper to settle it before the array is fixed.

How SUPERB PCBA settles the method

The method is reviewed with the array, not after it: outline shape, part distance to the cut, edge appearance, board thickness, copper weight and the volume the order is expected to run. Where two methods both work, the review says what each does to the edge and to the parts near it, and the customer picks with that in front of them.

Routing runs on RS-500 equipment, scoring to the limits above, and laser where the board calls for it. The array itself is covered in PCB panelization for assembly, the cost side in V-score and tab routing cost, and the keepout that separation needs in PCB edge clearance for assembly. Seven SMT lines run the first article on the machine that will build the order, so a method that damages parts shows up on one panel.

Questions buyers ask

Can one panel use two methods?

Yes. A common arrangement is a routed outline for the outer shape and a score between two identical boards. The second method costs a second tooling step, so it is worth it only where both are needed.

Does the method change the price of the bare board?

It changes tooling and machine time, not the laminate. The difference is small per board at volume and visible on a short run.

How close can a part be to a V-score?

Clear of the web and clear of the band that flexes when the panel is broken. The exact distance depends on thickness and on the part, and is settled per board.

Next step

Send the Gerber set, the panel drawing and the expected volume. The review comes back with the method that fits the outline and the parts, the limit it puts on part placement, and the tooling it needs, before the array is released.