Conformal coating looks like the simplest operation on a purchase order. The board is built, tested, coated and cured, and the price is usually a small fraction of the assembly. What the order rarely states is that coating is the last step where a good board can still be turned into a bad one.
Three things go wrong in that step, and all three are invisible at the moment they happen. Flux residue sealed under the film keeps working on the copper. Coating that wicks into a connector body fails at the customer's bench rather than on our line. A film that lands unevenly across a tuned microstrip moves the response of a filter trimmed before coating, and the board that passed no longer matches its own record.
So a coating job is a process question, not a spray question: material, keep clear areas, thickness and cure decide the result, and all four come from the customer's drawing.
Why a coating job fails on a board that already passed
Most coating failures start before the spray gun is switched on. Ionic residue from an incomplete wash sits under the film, and the film now holds that residue and moisture against the copper. Masking that is too small lets film creep onto a contact, and masking that is too large leaves bare copper where the drawing expected coverage.
Wetting is the second cause. Residue, hand grease or a badly cleaned solder mask repels the coating, and the film pulls back from the edge of a pad or a component body. The spot looks coated under normal light and shows as a bare island under ultraviolet.
Cure is the third. A film that is under cured stays tacky and collects dust. A film that is over cured becomes brittle and cracks at the corners of large components during thermal cycling. Both look identical on a shipping note.
What the coating drawing has to state
| Item | What has to be on the drawing | Why it decides the lot |
|---|---|---|
| Material family | Acrylic, silicone or polyurethane, with the data sheet and the qualification of that material | Sets the solvent, the cure window and the temperature range the film must survive |
| Keep clear areas | Connectors, test points, optical windows, press fit pins and any tuning structure the drawing names | Decides the masking job, and one missed area is a rework on a finished unit |
| Thickness | Target range, the surface it is measured on, and whether the value is wet or cured | A thickness read on the wrong surface passes a film that is thin over the joint |
| Cure | Temperature and time, or the ultraviolet dose, with the oven or lamp the process needs | Under cure leaves a tacky film, over cure cracks it in thermal cycling |
| Cleanliness before coat | The wash and the residue limit the board was built to | Coating over ionic residue traps the failure instead of preventing it |
| Acceptance | Inspection method, coverage class and the standard the lot is judged to | Decides whether a void in the film is a reject or an accepted condition |
How a coating lot runs at SUPERB PCBA
Coating sits at the end of the assembly flow, after reflow, after washing and after the functional check the build calls for. Boards are masked to the drawing, coated on a selective coating machine, cured in an ultraviolet and infrared oven, then inspected under ultraviolet before packing. Where the drawing calls for a measured film, thickness is read on the coupon it names.
The flow behind that station is seventeen steps with ten quality stations, held to IPC-A-610 Class 2 and Class 3, under ISO 9001 and ISO 13485 for medical work. Assembly runs on seven SMT lines with 01005 placement, 3D SPI after print, 3D AOI after reflow and X-ray read to IPC-7095 with voiding under five percent. Reflow is a twelve zone nitrogen oven under 500 ppm oxygen with SAC305.
The station itself is described under selective coating machine, the check under conformal coating inspection, and the material side under IPC-CC-830.
What coating does to an RF board and to a medical board
On an RF board the film is part of the electrical environment. A coating over a microstrip adds a dielectric layer whose thickness varies across the board, and a filter or a coupler trimmed in air will shift when that layer lands on it. The workable answer is to keep the tuning structures clear when the drawing allows it, and to coat and then re measure when it does not. Which structures are sensitive belongs on the drawing, not in a discussion after the fact. The assembly side of that kind of board is described under RF PCB assembly.
On a medical board the coating is a cleanliness decision as much as a protection decision. The film has to bond to a surface free of residue, so the wash before coating is part of the lot record. Medical builds run under ISO 13485, and biocompatibility and the sterilization route stay with the customer and their regulatory file. What we hold is the process: same material lot, same masking, same cure, and a record per lot.
On a military or outdoor build the film has to survive salt fog and thermal cycling, and failure usually starts at an edge where the film is thin. Edge coverage is a masking and spray path question, checked on the first article.
Conformal coating questions
Can you coat a board that has already been functionally tested?
Yes, and that is the usual sequence. Test before coating catches build defects while the board is still accessible. A second functional check after cure confirms that the film did not bridge a test point or load a sensitive node. Which tests run before and which after is agreed with the customer.
Do you choose the coating material for me?
Only when asked. If the drawing names a material, we buy it and keep the data sheet with the lot record. If the requirement is open, we propose two or three materials with their temperature range, solvent and cure, and the choice stays with the customer.
How are connectors and test points protected?
With masking, plugs and peelable mask applied to the keep clear list on the drawing. The check is visual and ultraviolet inspection after cure, and a masked area that shows film is a reject. This is the step where a short cut shows up months later at the customer's bench.
What happens to a board that fails the ultraviolet check?
It goes to a defined repair: a local strip and re coat of the affected area, or a full strip of the film, depending on the material and the drawing. A re coat is recorded as rework in the unit history and ships with that record.
Next step
Send the Gerber set, the coating drawing with the keep clear list, the material and the acceptance standard, or send a board that failed in the field together with the coating specified for it. The reply returns the masking plan, the material and cure route, the inspection method and a price with the coating listed as its own line.