The floor in IPC-6012 Class 3 is 50 micrometres of annular ring on an external plated through hole and 25 micrometres on an internal layer, measured after drilling and plating. That is a minimum to leave on the board, not a pad rule, and the two get mixed up on most drawings. A drawing that asks for 0.05 mm at a 0.3 mm via will produce a board with no ring at all at the worst case position on the panel, because the hole position tolerance alone is plus or minus 0.075 mm. The number that belongs on the drawing is the ring you want after misregistration, so the pad is the finished hole plus twice the ring plus twice the position tolerance.
Where the standard number comes from
IPC-6012 puts three figures in the same table: 50 micrometres for a supported external plated hole, 25 micrometres for an internal layer, and 150 micrometres for an unsupported hole, which is a hole with no copper land on the side the drill exits. Class 2 accepts a 90 degree breakout on external layers. Class 3 accepts no external breakout at all, and on internal layers it accepts a 90 degree breakout only while the land to conductor junction stays above the permitted width reduction.
The ring is not a feature that anyone adds. It is what remains when a hole is drilled through a pad and the barrel is plated, so three things decide it: where the drill lands, how much copper the plating puts on the barrel wall, and how far the laminate moved during lamination. IPC-6012 also asks for wrap plating to extend 25 micrometres onto the surface wherever a ring is required.
Why 50 micrometres is not a pad size
Four tolerances sit between the drawing and the cross-section. Hole position on our line is plus or minus 0.075 mm. A standard plated hole carries plus or minus 0.075 mm on finished diameter, and 0.05 mm when the pin is press-fit. Panel scale after lamination moves 0.03 to 0.05 mm across a 500 mm panel. Etch tolerance on the pad is plus or minus 20 percent of its width.
Add the first two and the arithmetic is simple. If registration can be 0.075 mm off and the ring still has to be 0.05 mm, the nominal ring has to be 0.125 mm, which means the pad is the finished hole plus 0.25 mm. For a 0.3 mm finished via that is a 0.55 mm pad. Most drawings carry 0.6 mm, and that is the only reason most boards pass.
| Finished hole | Minimum pad, Class 3 | Nominal ring | What drawings usually carry |
|---|---|---|---|
| 0.20 mm | 0.45 mm | 0.125 mm | 0.45 to 0.50 mm |
| 0.30 mm | 0.55 mm | 0.125 mm | 0.60 mm |
| 0.50 mm | 0.75 mm | 0.125 mm | 0.80 mm |
| 0.80 mm | 1.05 mm | 0.125 mm | 1.10 mm |
| 1.00 mm | 1.25 mm | 0.125 mm | 1.40 mm |
Component holes take more ring than vias, for mechanical reasons: a lead, a solder fillet and, sooner or later, a desoldering tool. Lifting a land with a vacuum tool at 300 degrees is a pull test on the barrel to land junction, and a 0.05 mm ring has a quarter of the junction area of a 0.2 mm ring. Our own process floor reflects that: 3.5 mil (0.089 mm) on a 1 oz via, 8.0 mil (0.203 mm) on a 1 oz component hole, and 4.5 mil and 10 mil once the copper goes to 2 oz.
What the ring does under thermal load
Copper expands at 17 ppm per degree and the laminate through its thickness runs at 50 to 70 ppm below Tg and around 200 ppm above it. Every reflow pass drives the barrel up and down against the land, and the junction between them is a right angle of plated copper about 20 micrometres thick. The ring is the area over which that movement is spread. A 0.05 mm ring spreads it over a fifth of the length of a 0.25 mm ring, so the shear per unit area at the knee is five times higher.
The failure starts as a circumferential crack at the knee of the barrel, grows with each cycle, and reads as an intermittent open that appears when the board is warm and disappears when it cools. Class 3 rejects a lifted ring for this reason alone. X-ray does not see it either, since the copper is still there but no longer attached: it takes a cross-section or a thermal cycle with resistance monitoring.
Three ways the number goes wrong
Writing 50 micrometres as a pad rule. The pad list comes out small, the board is cheap to route, and the first lot shows breakout on the vias near the panel edge, where drill position is worst. The ring on the drawing has to carry the position tolerance, or the breakout is built in.
Inheriting Class 2 acceptance under a Class 3 title block. It passes the fab audit and fails the customer audit. The class on the drawing governs breakout, plating thickness and lifted lands together. A board called Class 3 for plating thickness only, inspected to Class 2 breakout, is not a Class 3 board, and the ring is where the difference shows first.
Sizing 2 oz pads from the 1 oz table. Heavy copper needs 4.5 mil on a via and 10 mil on a component hole in our process, and the etch tolerance on a 2 oz pad is the same plus or minus 20 percent as on the trace. The pad that worked at 1 oz loses a third of its ring at 2 oz, with nothing changed except the copper weight.
What SUPERB PCB holds
Published figures for the FR-4 line: minimum annular ring 3.5 mil on a 1 oz via and 8.0 mil on a 1 oz component hole, hole position tolerance plus or minus 0.075 mm, plated through hole diameter plus or minus 0.075 mm and plus or minus 0.05 mm for press-fit, plating and hole wall copper 20 micrometres average, aspect ratio 10 to 1. Cross-sections report the measured ring at the tightest position of the panel, next to the drill position on the drawing.
The boundary is worth stating. Our hole wall copper is 20 micrometres average against the 25 micrometres that Class 3 asks for, so a Class 3 call-out goes through a process review before we accept the order. We do not quote a class we cannot hold in the cross-section, and a broken out ring is a reject, not a repair.
What to send with the drawing
Finished hole diameter and whether the figure is tool size or finished size, the class and whether breakout is acceptable on any layer, copper weight per layer, which holes take press-fit pins, whether any hole will be reworked in the field, and the panel outline if the board is small enough to sit near the panel edge. With those six items the pad table can be settled before the first panel, which is the only point where changing it costs nothing.