Half of the board is fine pitch parts on the underside, and the other half is a row of through-hole connectors that a harness will plug into. Running that panel straight over a wave puts the underside into molten solder at around 250 C, which is why the board travels through the machine inside a pallet: a machined carrier that covers what has to stay dry and opens only over the leads that have to be joined.

Wave solder pallet work is judged by what it lets through, not by what it covers. A pallet that masks a fraction of a millimetre too far leaves a lead with no fillet, and one that opens too wide lets solder reach a part that was never meant to see the wave.

What a pallet has to do on a mixed board

Four jobs, and they pull against each other. It has to hold the panel flat while it crosses the wave, so the board does not bow and lift a lead out of the solder. It has to shield every SMT area on the underside, including the parts that sit close to the through-hole row. It has to open a window over each lead that needs a fillet, with enough clearance for solder to flow and dross to leave. And it has to survive the machine, panel after panel, without the openings growing or the surface charring through.

The features that decide the joint

FeatureWhat it is set againstWhat goes wrong outside it
Material and thicknessBoard size, wave width, and the preheat the joints need before they reach the solderA thin pallet bows across the wave and lifts the last row of leads; a thick one keeps preheat from reaching the barrels
Opening sizeLead diameter plus clearance on each side, enough for a fillet and for dross to clearToo tight masks the fillet on one side, too wide puts solder on a neighbouring SMT pad
Wall between openingsPad pitch on the connector and the step that holds the board downA thin wall erodes first and the opening widens over the life of the pallet
Hold-downClamps or spring fingers placed where they do not sit on a partA panel that lifts a fraction of a millimetre gives a partial fillet on the trailing edge
Fingers and edge clearanceConveyor width and the shadow cast behind each fingerSolder cannot reach a joint standing in the shadow, and the result looks like a cold joint
IdentificationPallet number and revision marked on the frame, away from the wave contact areaTwo pallets in circulation with different openings is the classic mixed-up build

These are starting values, not settings. What decides whether a pallet is right is the fillet on the first article, read against the acceptance class, plus a cut through a barrel when the fill is in question.

Three failures a pallet causes

The first is a masked fillet. The opening is a little small or sits a little off the lead, and the joint forms on three sides with the fourth covered. It passes a quick look because there is solder on the pad, and it fails a thermal cycle because the barrel is not filled.

The second is shadowing. A finger, a wall or a clamp stands between the lead and the wave and the solder never arrives. The joint looks cold and is actually unfilled, so it gets chased in the profile when the answer is in the pallet.

The third is flooding. The opening is generous or the wall has eroded, and solder crosses onto the SMT side. With 0402 parts near the connector row that is not a touch-up, it is a rework with hot air on parts that were already inspected.

How a pallet ages

Composite pallets erode where the wave touches them. Opening edges round over and the surface chars. A pallet that has run a few thousand panels is not the pallet that was qualified, even though it looks the same on the bench. Wear shows up first as a fillet that gets smaller on one side of a connector, then as solder on a pad that used to be covered.

The control is a pallet number, a running count, and a check of the opening edges at a set interval.

When a pallet is the wrong answer

Boards with a high through-hole count, connectors with heavy thermal mass, or parts that cannot see 250 C at all are poor candidates. On those the joints are made one at a time with a nozzle, which keeps the rest of the board at room temperature. That path is on selective soldering process.

A board with a handful of leads and a dense underside sometimes runs better with paste printed over the holes and the connector reflowed with everything else, so no separate wave step is needed. That is on pin in paste through hole assembly.

How SUPERB PCBA runs a pallet build

Wave work runs on the JT-450 and JT-350 machines, with the pallet cut to the panel outline and to the connector positions on the assembly drawing. The SMT side is built first on one of seven SMT lines, with placement to 01005 (0.4 by 0.2 mm) at up to 40,000 CPH, and the print is checked on 3D SPI before any part is placed, so the underside is verified while it can still be corrected.

Reflow runs on a twelve zone nitrogen oven at under 500 ppm oxygen with a SAC305 profile, and the wave that follows is judged on the through-hole fill and the fillet, with optical inspection after and X-ray where a barrel is not visible. Acceptance is to IPC-A-610 Class 2 or Class 3 as the drawing states. The pallet is proven on the first panel, and the openings and wave parameters are recorded against the pallet number.

What to send with a mixed board

Four things shorten the first article: the Gerber set, the BOM, an assembly drawing with the through-hole parts marked and their side noted, and the connector drawings with pin length and body height. A note on any part that must not see the wave drives where the walls go. The pallet comes back as a drawing for approval before anything is cut, with the openings, the walls and the hold-down points shown against the board outline.

Questions buyers ask

Does the pallet change the wave profile?

Yes. The pallet is thermal mass under the board, so preheat takes longer to reach the barrels and the contact time is set with the pallet in place, not on a bare panel.

How is a masked fillet corrected?

By opening the window or moving the wall, not by raising the solder temperature. A hotter wave on a masked joint gives a dirtier connector and the same missing fillet.

Next step

Send the BOM, the Gerber set and the assembly drawing with the through-hole parts marked. The reply comes back with the pallet drawing for approval, the wave parameters the first article will run at, and the joints that will be cut and measured to prove the fill.